IMMERSION IRON PHOSPHATE PROCESS LINE

DEGREASING RINSING RINSING IRON PHOSPHATING RINSING PASSIVATION DRYING
temp. : 70-90 ºC temp. : 50-60 ºC temp. : 20-60 ºC temp :max.120 ºC
time : 5-15 min. time : 5-8 min. time : 0.5-2 min.
tank : can be DKP. tank : stainless. tank : stainless.


![]()
![]()
![]()
![]()
![]()
![]()